Dec 19, 2025 Lasciate un messaggio

ASME B16.11 Threaded 90 Degree Elbows Dimension

ASME B16.11 Threaded 90℃ Elbows are crucial pipe fittings in piping systems for achieving a 90℃ change in fluid direction. They connect to pipes via internal or external threads at both ends, eliminating the need for welding and offering easy assembly and disassembly. They are widely used in applications such as petroleum, chemical, natural gas, and civil water supply and drainage systems that require frequent maintenance or operate under low-pressure conditions.

 

HT PIPE is a leading stockist and global exporter with over 15 years of expertise in international trade. We supply pipes, plates, round bars, and a comprehensive range of pipe fittings, flanges, and valves. now for free quotes and personalized product information.

 

Refers to the outer diameter of the elbow's connection end after beveling. This dimension must match the outer diameter of the connecting pipe.

Center-to-End Dimension: Refers to the perpendicular distance from the centerline of the elbow to the end face of either port. This is a critical dimension for determining the pipe layout space. ASME B16.11 90℃ elbows are typically short-radius type, with a smaller center-to-end dimension, facilitating installation in confined spaces.

ASME B16.11 threaded elbows typically use American Standard tapered pipe threads. A minimum thread length is required to ensure sufficient engagement length for effective sealing.

threaded 90℃elbows

A

H

G

L5

L2

90℃ Elbows tees Crosses

45℃ Elbows

2000

3000

6000

2000

3000

6000

2000

3000

6000

2000

3000

6000

6

1/8

21

21

25

17

17

19

22

22

25

3.18

3.18

6.35

6.4

6.7

8

1/4

21

25

28

17

19

22

22

25

33

3.18

3.30

6.60

8.1

10.2

10

3/8

25

28

33

19

22

25

25

33

38

3.18

3.51

6.98

9.1

10.4

15

1/2

28

33

38

22

25

28

33

38

46

3.18

4.09

8.15

10.9

13.6

20

3/4

33

38

44

25

28

33

38

46

56

3.18

4.32

8.53

12.7

13.9

25

1

38

44

51

28

33

35

46

56

62

3.68

4.98

9.93

14.7

17.3

32

11/4

44

51

60

33

35

43

56

62

75

3.89

5.28

10.59

17.0

18.0

40

11/2

51

60

64

35

43

44

62

75

84

4.01

5.56

11.07

17.8

18.4

50

2

60

64

83

43

44

52

75

84

102

4.27

7.14

12.09

19.0

19.2

65

21/2

76

83

95

52

52

64

92

102

121

5.61

7.65

15.29

23.6

28.9

80

3

86

95

106

64

64

79

109

121

146

5.99

8.84

16.64

25.9

30.5

100

4

106

114

114

79

79

79

146

152

152

6.55

11.18

18.67

27.7

33.0

 

 

 

Invia la tua richiesta

whatsapp

Telefono

Posta elettronica

Inchiesta